1040, 1045 (HR,CF) - Used when greater strength and hardness is desired in the as rolled condition. Good for hammer forge processes. Uses include gears, shafts, axles, bolts sand studs. 1040 is a medium-carbon steel composed of 0.37 to 0.44 percent carbon, 0.6 to 0.9 percent manganese, a maximum of 0.04 percent phosphorus and a maximum of 0.05 sulphur. The remainder is iron. 1040 steel sometimes contains 0.1 to 0.35 percent silicon, according to Interlloy, an Australia-based alloy engineering steel, tool steel and specialty steel producer.

AISI 1040 equivalent to EN8/080M40. An unalloyed medium carbon steel. AISI 1040 is a medium strength steel with good tensile strength. Suitable for shafts, stressed pins, studs, keys etc. 1040 must be pre-heated to 300 to 500 degrees F before welding and reheated to between 1100 degrees F and 1200 degrees F after welding. Otherwise, the area near the weld may develop cracks or become brittle and cause the part to fail during use.

Tensile Strength
Ultimate tensile strength is the maximum load a material will support before it breaks, explains Instron, a materials testing laboratory. Ultimate tensile strength testing is a destruction test. The purpose is to find the point at which a material will fail when supporting a given load or sustaining a set force.

1040 steel will support 90,000 pounds of force per square inch before it fails, if it was hot-rolled. This strength drops to 85,500 psi when the steel has been normalized, or returned as closely as possible to the state it was in when it was produced. Tensile strength drops even further, to 72,250, when it has been annealed, or brought to its softest point while cold.



Normalizing and annealing are two examples of heat treatments. In heat treatment the temperature of the steel is changed in order to alter its molecular structure and change its reaction to various forces during forging and fabrication, according to metallurgist David Pye's heat treatment tutorial at Moldmaking Technology.

Ductility
Ductility is the ability of a material to change shape under stress and force without breaking. It is also a measure of how far a material will stretch or spread under force before it cracks or flakes. The more ductile a metal is, the easier it is to deform and reform without applying heat. Automakers take advantage of the ductility of steel when they build in what are called "crumple zones." These are parts of a car that are intentionally designed to crumple under force, absorbing impact and preventing injury to the driver and passengers.

1040 steel can be deformed to just under 28 percent of its original dimensions with a 54.9 percent reduction in area. Reduction in area is the difference between the original piece prior to testing and the minimum area after the break divided by the area of the original piece.

Principal Design Features
1040 steel has a higher (0.40%) carbon content for greater strength than the lower carbon alloys. It is hardenable by heat treatment, quench and tempering to develop 150 to 250 ksi tensile strength.

Applications
Used for crankshafts, couplings and cold headed parts.

Machinability
Machinability is good, rated at 60% that of the 1112 alloy used as a 100% machining rated steel.

Forming
Forming of 1040 steel in the annealed condition is readily accomplished.

Welding
1040 steel is weldable by all of the welding methods. However with its higher carbon content it is important to use both pre-heat at 300 to 500 F and post-heat at 1100 to 1200 F practice per an approved welding procedure.




Heat Treatment
This steel responds well to hardening by heat treatment at 1550 to 1650 F followed by water quench and then tempering to strength level desired.

Forging
Forge at 2300 F down to 1800 F.

Hot Working
Hot work from 900 to 200 F.

Cold Working
In the annealed state the 1040 alloy is readily cold worked by conventional methods.

Annealing
Anneal at 1600 to 1800 F and slow cool in the furnace for a full anneal. A stress relief anneal may be done at 1100 F and a normalizing treatment may be done at 1650 F with slow cooling.

Tempering
Tempering from the quenched condition may be done at 600 to 1300 F depending upon the strength desired.

Hardening
Cold work will harden the alloy as will heat treatment and tempering.

AISI BS 970 1955 EN BS 970 1991 Werkstoff
1040 EN8 080M40 1.1186

Chemical Composition
Carbon 0.37 - 0.44
Iron Balance
Manganese 0.6 - 0.9
Phosphorus 0.04 max
Sulphur 0.05 max
Physical Data
Density (lb / cu. in.) 0.284
Specific Gravity 7.86
Specific Heat (Btu/lb/Deg F - [32-212 Deg F]) 0.107
Melting Point (Deg F) 2770
Poissons Ratio 0.3
Thermal Conductivity 360
Mean Coeff Thermal Expansion 6.7
Modulus of Elasticity Tension 30
Modulus of Elasticity Torsion 11
Mechanical Data
Form Round Bar
Condition Cold Drawn
Temper 68
Tensile Strength 85
Yield Strength 71
Elongation 17
Reduction of Area 42
Rockwell B93
Brinnell 170
Form Round Bar
Condition Hot Rolled
Temper 68
Tensile Strength 90
Yield Strength 56
Elongation 24
Reduction of Area 49
Rockwell B91
Brinnell 187

1008 | 1010 | 1015 | 1018 | 1020 | 1025 | 1035 | 1040 | 1045 | 1050 | 1117 | 1141 | 1144 | 12L14 | 1215 | 4140 | 4150 | 4340 | 8620 | A36 | A653 | A513 | Mechanical Properties | Physical Properties | Carbon Steel Pipe Standards | ASTM A53 B Working Pressure | ASTM A106 B Pressure Temperature Rating | Carbon Steel | Steel Alloy Designations | Chemical Composition Analysis of Carbon Steel Table | UNS Number G1 | UNS Number G2 | UNS Number G3 | UNS Number G4 | UNS Number G5 | UNS Number G6 | UNS Number G7

Pipes Tubes Plates Bars Square Tubes Weight Calculation Calculator
Pipe Working Pressure Calculation
Conversion Calculator Calculation-Pressure|Weight|Temperature|Volume|Length
Conversion Table-Pressure|Stress|Mass|Length|Temperature|SI Prelxes
Metals Weight Calculator-Aluminum|Brass|Bronze|Copper|Magnesium|Plastic|Nickel|Stainless Steel|Steel|Titanium|Zinc


stainless steel pipe AISI Steel Mechanical Characteristics - Yield Tensile Elongation Hardness
Direct contact heat exchanger
How to detect the hardness of stainless steel pipe
Super-Duplex Stainless Steels and their characteristics
Compression Testing
Bend Testing
The Difference Between Yield Strength and Tensile Strength
ASTM A556M ASME SA556 Seamless cold drawn steel feedwater heater tubes
Intergranular Corrosion
Select Materials for Heat Exchanger Tubes with Substantial Pressure difference
EN 10088-1 Elevated temperature physical properties of stainless steel
EN 10088-1 Ambient temperature physical properties of stainless steel
Selection of Stainless Steel from Corrosion Resistance, Mechanical Physical Properties Forming,Fabrication Joining
BSEN ASTM British and American standards for tolerances, surface finish and testing of stainless steels
Stainless Steel Cold Working Properties
Stainless Steel Relative Cost Data
Heat Treating Stainless Steel | Heat treatment Stainless Steel
High Temperature Stainless Steel
Chloride Stress Corrosion Cracking Stainless Steel
ASME Specifications Stainless Steel FORGINGS BOLTING PLATE SHEET STRIPCASTINGS PIPING TUBING Tube Pipe BARS SHAPES
Seawater Resistance of Stainless Steel
Properties at Cryogenic Temperatures of Stainless Steel Tubes
Intergranular Corrosion of Stainless Steel Tubes
Cleaning of Stainless Steel Tubes
stainless steel pipe DIN 2391. Seamless Precision Steel Tubes
stainless steel pipe DIN 2393. Welded Precision Steel Tubes
stainless steel pipe DIN 2394. As-Welded and Sized Precision Steel Tubes
stainless steel pipe DIN 2395. Rectangular and Square Welded Precision Steel Tubes
stainless steel pipe DIN 2440 & DIN 2441. Steel Tubes; Medium-Weight Suitable for Screwing & Heavy-Weight Suitable for Screwing
stainless steel pipe DIN 17175. Seamless Tubes of Heat-Resistant Steels
stainless steel pipe DIN 17458/2462. Seamless Circular Tubes of Austenitic Stainless Steels with Special Quality Requirements
stainless steel pipe ASTM A 53 & ASTM A 106. Welded and Seamless Black Pipes & Seamless Pipes from Carbon Steel, Intended for Operation by High Temperature
stainless steel pipe ASTM A213/A450. Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat Exchanger Tubes
stainless steel pipe ASTM A312/A999. Seamless Austenitic Stainless Steel Pipes
stainless steel pipe API 5L. Line Pipes
stainless steel pipe API 5CT. Tubings
stainless steel pipe GOST 800-78. Bearing Tubes
stainless steel pipe GOST 949-73. Small and Medium Volume Steel Cylinders for Gases
stainless steel pipe GOST 949-73 & TU 14-3R-10-94. Steel Cylinders of Medium Volume with Concave Bottom for Gases
stainless steel pipe GOST 3262-75. Water-supply and Gas-supply Steel Pipes
stainless steel pipe GOST 8639-82. Square Steel Pipes
stainless steel pipe GOST 8645-68. Rectangular Steel Tubes
stainless steel pipe GOST 8732-78. Seamless Hot-Formed Steel Pipes
stainless steel pipe GOST 8734-75. Seamless Steel Tubes Cold-Formed
stainless steel pipe GOST 9940-81. Seamless Cold-Finished and Warm-Finished Tubes of Corrosion Resistant Steel
stainless steel pipe GOST 9941-81. Seamless Cold-Finished and Warm-Finished Tubes of Corrosion Resistant Steel
stainless steel pipe GOST 10704-91. Electrically Welded Steel Line-End Tubes
stainless steel pipe GOST 14162-79. Steel Tubes of Small Dimensions (Capillary)
stainless steel pipe GOST 19277-73. Seamless Steel Tubes for Oil and Fuel Lines
stainless steel pipe TU 14-159-263-96. Electrically Welded Cold-Formed and Seamless Precision Steel Pipes for Automotive Industry
UNS Number S4 GROUP Heat and Corrosion Resistant Steeels (Including Stainless), Valve Steels, and Iron Baes "Super alloys")
ASTM A789-A789M SEAMLESS AND WELDED FERRITIC/AUSTENITIC STAINLESS STEEL TUBING FOR GENERAL SERVICE
ASTM A213M/ASME SA213 SEAMLESS FERRITIC AND AUSTENITIC ALLOY STEEL BOILER SUPERHEATER AND HEAT EXCHANGER TUBES
ASTM A312/ASME SA312 SEAMLESS AND WELDED AUSTENITIC STAINLESS STEEL PIPE
A 269-04 Standard Specification for Seamless and Welded Austenitic Stainless Steel Tubing for General Service
ASTM A376M-8/ASME SA376 SEAMLESS AUSTENITIC STEEL PIPE FOR HIGH TEMPERATURE CENTRAL STATION SERVICE
ASTM A 511/A 511M Standard Specification for Seamless Stainless Steel Mechanical Tubing
ASTM A 790/A 790M Standard Specification for Seamless and Welded Ferritic/Austenitic Stainless Steel Pipe