Solution Annealing - Heat to 815-845°C, hold for ½ hour per 25mm of thickness, slow furnace cool to 600°C and then quickly air cool. Slow cooling from 540-400°C will cause embrittlement.

Sub-Critical anneal - Heat to 760-815°C and then air cool or water quench.

This grade is not hardenable by thermal treatment.

Note that 430 is likely to scale more heavily at elevated temperatures than 304, and the scale produced is more difficult to remove by pickling.

Back to 430

Applications
Standard Specification
Chemical Composition
Grade Comparison
Corrosion Resistance
Heat Resistance
Physical Properties
Mechanical Properties
Thermal Processing
Heat Treatment
Welding
Machining
304/304L/304LN/304H Tubing and Pipe

430 Stainless Steel Tube | 430F Stainless Steel Pipe


304 | 304L | 304H | 316/316L | 316Ti | 317L | 321/321H | 309S | 310S | 347/347H | S32205/S31803 | S32304 | S32750 | S32760 | 904L | 405 | 410 | 410S | 430

    © Copyright Reserved   Home  |  Site Map   |  Links  |  Directory  |  Advertise  |   Heat  |  Tools  |  Standard  |  Pressure  |  Hardness  |  Surface   |  Metal Engineering
     E-mail: sales@stainless-steel-tube.org                                        
    Stainless Steel Pipe | Stainless Steel Tube | Stainless Steel Tubing | Heat Exchanger Tube | Duplex Stainless Steel Pipe | U Bend Tube